Through hardening steels

ARMAD

Spécifications

EU
32CrMoV12-10

Composition

C
0.32
Cr
3.1
Mo
1
V
0.3

Applications

• Gun barrels for firearms when a balance between ultimate tensile strength (UTS) and Impact Toughness (KV) at -40°C is above standard used steel grades.
• For any safety mechanical application for which a balance between strength and impact toughness is needed expecially at low temperatures.

Characteristics

• Very good ability to cold hammering and button rifling.
• Opportunity to heat treat above 40 HRC, while maintaining a high level of Charpy Impact Toughness at 20°C and -40°C, enhancing firearm performances in operation.

Mechanical properties

Heat
treatment
UTS
(N/mm²)
0,2%
YS
(N/mm²)
A
(%)
KV
(J)
T + Rv 570°C 1500 1300 15 80
T + Rv 610°C1250105020200

Key to heat treatment symbols

Solution treated H Annealed R
Thermo-mechanical treatment TM Quenched and tempered T+RV
Sub-zero treatment F Solution treated and aged H+V

See also

GKH

Steels for nitriding