ARMAD Through hardening steels
Spécifications
- EU
32CrMoV12-10
Typical composition
- C
0,32
- Cr
3,1
- Mo
1
- V
0,3
Applications
• Gun barrels for firearms when a balance between ultimate tensile strength (UTS) and Impact Toughness (KV) at -40°C is above standard used steel grade and good wear erosion.
• For any safety mechanical application for which a balance between strength and impact toughness is needed expecially at low temperatures.
Mechanical properties
• Very good ability to cold hammering and button rifling.
• Opportunity to heat treat above 40 HRC, while maintaining a high level of Charpy Impact Toughness at 20°C and -40°C, enhancing firearm performances in operation.
Mechanical features
Heat treatment | UTS (N/mm²) | A (%) | KV -60°C (J) |
---|---|---|---|
T + Rv 600°C | 1400 | 17 | 110 |
T + Rv 620°C | 1220 | 19 | 180 |
- Solution treated : H
Annealed : R - Thermo-mechanical treatment : TM
Quenched and tempered : T+RV - Sub-zero treatment : F
Solution treated and aged : T+RV